Grain Specifications LEP
Classes – LEP Wheat
- CWSWS
- CPSR
- CWSP
- CWRW
- CWRS
- CWAD
Specifications
- Minimum 58 lbs/bu or 352g/0.5 litre (Avery Scale)
- Light weight discounted 2% dockage for each pound under 58 down to 54
- Maximum Moisture 15.0% (No discount)
- Moisture 15.1% to 16.0% discounted 3.0% dockage
- Moisture 16.1% to 17.0 discounted 6.0%
- Maximum 10.0% sprouted
- Maximum 3.0% mixed cereals
- Maximum .06% ergot (No discount)
- Ergot 0.07% to 0.09% discounted 3.0%
- Ergot 0.10% to 0.12% discounted 6.0%
- Maximum 2.0% heated
- No excreta
- No mould
- Maximum 1.0 ppm vomitoxin
- Maximum 5.0% actual dockage
Specifications � LEP Corn
- Minimum 53 lbs/bu or 333g/0.5 litre (Avery Scale)
- Weight 51.0 lbs (320g/ 5 L) to 52.9 lbs (332 g/.5L) discounted 2.0% dockage
- Weight 49.0 lbs (307g/5 L) to 50.9 lbs (319 g/.5L) discounted 4.0% dockage
- Maximum Moisture 15.5%
- Moisture 15.6 % to 16.0% discounted 3% dockage
- Moisture 16.1 % and higher subject to rejection
- Maximum 2.0% heated (included in total damaged)
- Maximum 5.0% damaged
- Maximum 3.0% cracked corn and foreign material
- Maximum 1.0 ppm vomitoxin
- No other cereal grains
Specifications subject to change at anytime.
Loads that do not meet these specifications will be rejected.